NOMINAL DATA SHEET
|
ALLOY 52 TYPICAL NOMINAL CHEMISTRY
|
|
|
ALLOY 52 TYPICAL TENSILE STRENGTH
|
|
|
|
NICKEL (NI)
|
50.5
|
ANNEALED
|
85,000 MAX.
|
|
CHROMIUM (CR)
|
0.10
|
1/4 HARD
|
90,000 to 115,000
|
|
MANGANESE(MN)
|
0.60
|
1/2 HARD
|
105,000 to 125,000
|
|
SILICON (SI)
|
0.30
|
HARD
|
120,000 MIN.
|
|
CARBON (C)
|
0.05
|
|
|
ALUMINUM (AL)
|
0.10
|
TYPICAL HARDNESS, ROCKWELL B
|
|
MAGNESIUM (MG)
|
0.50
|
ANNEALED
|
70 MAX.
|
|
ZIRCONIUM (ZR)
|
0.00
|
1/4 HARD
|
78 to 83
|
|
TITANIUM (TI)
|
0.00
|
1/2 HARD
|
84 to 88
|
|
PHOSPHORUS (P)
|
0.025
|
|
|
|
SULFUR (S)
|
0.025
|
|
|
|
IRON
|
BALANCE
|
|
|
|
|
|
TYPICAL LINEAR COEFFICIENT OF THERMAL EXPANSION (cm. per cm. C x 10 - 6)
|
|
30 to 100
|
10.5
|
|
30 to 200
|
10.4
|
|
30 to 300
|
10.2
|
|
30 to 350
|
10.2
|
|
30 to 400
|
10.1
|
|
30 to 425
|
N/A
|
|
30 to 450
|
10.1
|
|
30 to 500
|
10.0
|
|
30 to 550
|
10.5
|
|
30 to 600
|
10.8
|
|
30 to 700
|
11.7
|
|
30 to 800
|
12.5
|
|
30 to 900
|
13.3
|
|
30 to 1000
|
14.2
|
|
|
|